Chemical composition
 
    
    
 | C(%) | P(%) | N(%) | S(%) | Thick (mm) | Yield stress (Mpa) | Tensile stress (Mpa) |  |  |  | 
≦0.21 | ≦0.21 | ≦0.21 | ≦0.21 | ≦0.21 | ≦0.21 | ≦0.21 | ≦0.21 | ≦0.21 | ≦0.21 | 
 
Applications
Rolled Steels for Welded Structure 
Country Code:
 DIN
Standard
  17100
Steel Type 
  St44-2
Heat treatment 
Heat Treatment of steel grade St44-2
Heat treated : 1491°C - 1589°C
 
 
Relate Steel Type 
    
    
 | Inquiry | Steel Type | Standard | Country Code | C(%) | Si(%) | Mn(%) | P(%) | N(%) | S(%) | 
 |  |  |  |  |  |  | ≦0.035 |  | ≦0.035 |  | SM400B | 2947 | CNS | ≦0.20 | ≦0.35 | 0.60-1.40 | ≦0.035 |  | ≦0.035 |  | Q235B | T700 | GB | 0.12-0.20 | ≦0.30 | 0.30-0.70 | ≦0.035 |  | ≦0.035 |  | SM400B | G3106 | JIS | ≦0.20 | ≦0.35 | 0.60-1.40 | ≦0.035 |  | ≦0.035 |  | Gr.D | A284 | ASTM | ≦0.27 | 0.15-0.40 | ≦0.90 | ≦0.035 |  | ≦0.035 |  | RSt42-2 | 17100 | DIN | ≦0.25 |  | 0.20-0.50 | ≦0.035 |  | ≦0.035 |  | St42-3U | 17100 | DIN | ≦0.23 | 0.03-0.30 | 0.20-0.50 | ≦0.035 |  | ≦0.035 |  | St44-2 | 17100 | DIN | ≦0.21 |  |  | ≦0.035 |  | ≦0.035 |  | St44-3 | 17100 | DIN | ≦0.20 |  |  | ≦0.035 |  | ≦0.035 |  | Q255A | T700 | GB | 0.18-0.28 |  | 0.40-0.70 | ≦0.035 |  | ≦0.035 |  | Q255B | T700 | GB | 0.18-0.28 |  | 0.40-0.70 | ≦0.035 |  | ≦0.035 |  | SM400A | G3101 | JIS | ≦0.23 |  | ≧2.50 | ≦0.035 |  | ≦0.035 |  | SM400B | G3101 | JIS | ≦0.20 |  | 0.60-1.40 | ≦0.035 |  | ≦0.035 |  | Gr.36 | A709M | ASTM | ≦0.26 |  |  | ≦0.035 |  | ≦0.035 |